LED production process
Date:2011-04-13 15:17
Status:Close
Question:admin
thawing about thirty minutes, security thawed then Mix (20-30 minutes)
Silver plastic before the height of chips 1 / 3, up to 1 / 4 , the eccentric distance is less than 1 / 3 the diameter of the chip
Third step:Solid crystal
Solid crystal pen with solid crystal plane to maintain 30-45 degrees Celsius. forefinger down to the tip top
Solid crystal in order from top to bottom, left to right
Crystal pen with solid crystalline cements to frame, wrist insulated plastic center
Forth step:Solid crysta