General requirements:
a. purpose
b. scope of use
c. use of equipment
d,documents
e. operating standards
f, notes
g. quality requirements
First step:stent row
Before the step: expanding crystal
Temperature: 50-60 degrees Celsius, warm-up about ten minutes,when expand the temperature is set to 65-75 degrees Celsius.
Second step:. point glue
Adjust time of point glue 0.2-0.4 seconds ;Barometer knob 0.05-0.52mPa;adjust the dispensing knob resorted to plastic standard
Remove the plastic from refrigerator, thawing about thirty minutes, security thawed then Mix (20-30 minutes)
Silver plastic before the height of chips 1 / 3, up to 1 / 4 , the eccentric distance is less than 1 / 3 the diameter of the chip
Third step:Solid crystal
Solid crystal pen with solid crystal plane to maintain 30-45 degrees Celsius. forefinger down to the tip top
Solid crystal in order from top to bottom, left to right
Crystal pen with solid crystalline cements to frame, wrist insulated plastic center